Molding Process 7 visualizações

HDPE product low-temperature brittle cracking

Fenómeno do problema
HDPE products crack when used in winter.
Análise das causas
HDPE has high crystallinity and reduced low-temperature toughness; notch-sensitive, sharp corners easily crack at low temperature.
Solução
①Select high-impact grades for low-temperature applications; ②eliminate sharp corners in the structure; ③conduct low-temperature drop verification; ④avoid large deformation assembly at low temperature.
Conclusão principal
Low-temperature applications: grade selection + rounded corners as double insurance.