HDPE film poor corona treatment
Problembeschreibung
Poor corona treatment effect before printing, poor ink adhesion.
Ursachenanalyse
Corona power/speed mismatch, electrode contamination, slip agent migration on the film surface hindering the treatment effect.
Lösung
①Calibrate corona power and speed; ②clean the electrodes; ③evaluate slip agent migration; ④print promptly after treatment.
Wichtigste Erkenntnis
Corona effect = power + cleanliness + timeliness.