HDPE storage management
Problembeschreibung
Bubbles appear during processing after HDPE pellets are stored open
Ursachenanalyse
Surface-attached water accumulates, especially in powder and recycled material; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Lösung
Store pellets sealed; dry recycled material; first in first out; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, to facilitate locating effective measures
Wichtigste Erkenntnis
HDPE storage: sealed, first in first out; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar future problems
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!