Processing Machinery 6 Aufrufe

HDPE Stress Cracking

Problembeschreibung
HDPE container cracks after holding detergent
Ursachenanalyse
HDPE environmental stress cracking resistance (ESCR) is limited, and surfactants induce cracking; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based solely on experience
Lösung
Select high-ESCR grades; design the container structure to reduce stress; verify medium compatibility; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Wichtigste Erkenntnis
HDPE stress cracking is selected and verified according to ESCR; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
HDPEESCRstress crackingmedium