HDPE Stress Cracking
Fenómeno do problema
HDPE container cracks after holding detergent
Análise das causas
HDPE environmental stress cracking resistance (ESCR) is limited, and surfactants induce cracking; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based solely on experience
Solução
Select high-ESCR grades; design the container structure to reduce stress; verify medium compatibility; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
HDPE stress cracking is selected and verified according to ESCR; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!