Molds & Tooling
3 Aufrufe
LDPE Film Die Cavity Debris Streaks
Problembeschreibung
Continuous longitudinal streaks at a fixed position on the film surface, which disappear after cleaning the die.
Ursachenanalyse
Debris in the die cavity disturbs local melt flow causing uneven output; degraded hang-up material also forms persistent streaks.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
Lösung
①Regularly clean the die and die cavity; ②Check the screen to prevent impurity entry; ③Control temperature to reduce degraded hang-up material; ④Disassemble and polish the die when necessary.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Wichtigste Erkenntnis
Fixed-position streaks are the fingerprint of a local die cavity problem; establishing a regular cleaning system can prevent recurrence.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!