LLDPE material changeover cleaning
Problembeschreibung
After switching between LDPE and LLDPE, not switching process parameters causes batch defects
Ursachenanalyse
LDPE and LLDPE differ greatly in rheological properties: die gap, air ring type and temperature settings are all different; changing material without changing parameters inevitably causes melt fracture or bubble instability
Lösung
①After material changeover, switch the full set of die gap, air ring and temperature; ②archive and recall parameters by material type; ③downgrade and isolate transition-period products; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
LDPE and LLDPE changeover is a full parameter switch; die gap, air ring and temperature are three linked items, none can be omitted; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!