Sorun Belirtisi
After switching between LDPE and LLDPE, not switching process parameters causes batch defects
Neden Analizi
LDPE and LLDPE differ greatly in rheological properties: die gap, air ring type and temperature settings are all different; changing material without changing parameters inevitably causes melt fracture or bubble instability
Çözüm
①After material changeover, switch the full set of die gap, air ring and temperature; ②archive and recall parameters by material type; ③downgrade and isolate transition-period products; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Temel Çıkarım
LDPE and LLDPE changeover is a full parameter switch; die gap, air ring and temperature are three linked items, none can be omitted; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
Bu faydalı oldu mu?
0 kişi bunu faydalı buldu
Geri bildiriminiz için teşekkürler!