Molds & Tooling 3 Aufrufe

LLDPE Ejection Whitening

Problembeschreibung
LLDPE product whitens at ejector pin positions
Ursachenanalyse
Stress concentration during ejection; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based solely on experience; This mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Lösung
Larger and more ejector pins; sufficient cooling; sufficient draft angle; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; Change only one variable at a time and record parameter changes to facilitate locating effective measures
Wichtigste Erkenntnis
Ejection whitening relies on balanced ejection; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; Include this case in the defect archive as a troubleshooting reference for subsequent similar problems
LLDPEejection whiteningejector pincooling