Material Drying
3 Aufrufe
PA12 Product Embrittlement and Fracture
Problembeschreibung
The product breaks brittlely under stress, more severe at low temperature.
Ursachenanalyse
Material degradation or insufficient drying reduces molecular weight; PA12 itself has good low-temperature toughness but is still sensitive at notches; excessive shear also reduces toughness.; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based solely on experience
Lösung
①Control processing temperature to prevent degradation; ②sufficient drying; ③avoid sharp corners and notches in structure; ④select toughened grade for verification.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
For PA12 embrittlement, check degradation and moisture; structural design cooperates with material protection.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; Include this case in the defect archive as a troubleshooting reference for subsequent similar problems
War das hilfreich?
0 Personen fanden dies hilfreich