PA6 Product Hydrolysis Resistance Requirement Failure

Problembeschreibung
PA6 parts used in humid and hot environments degraded rapidly in performance and strength declined.
Ursachenanalyse
Ordinary PA6 has limited hydrolysis resistance, and molecular weight declines under long-term humidity and heat; hydrolysis-resistant grades should be selected; humid and hot environments are a severe test for ordinary PA6; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience.
Lösung
①Select hydrolysis-resistant modified grades for humid and hot uses;②perform humid heat aging verification;③leave performance margin in design;④do a good job of sealing and moisture-proofing, and control environment and storage humidity;⑤evaluate alternative materials.
Wichtigste Erkenntnis
PA6 'humid and hot environment = hydrolysis-resistant grade threshold': ordinary nylon cannot withstand long-term humidity and heat; the environment must be matched at the material selection stage, and post-remediation is ineffective; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence.
PA6; hydrolysis resistance; humid heat aging; grade