Material Drying 7 Aufrufe

PA66 product drop fracture

Problembeschreibung
Drops fracture along weld lines, test failed.
Ursachenanalyse
Weak weld lines + dry-state brittleness; sharp corner concentration also does; the fracture path points to the root cause; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience.
Lösung
①Adjust the gate so weld lines avoid the stress path; ②condition before assembly to restore toughness and stabilize dimensions; ③change sharp corners to rounded transitions to eliminate stress concentration; ④strengthen drying and verify moisture content compliance by moisture determination; ⑤structurally reinforce weak parts (fillets, reinforcing ribs).
Wichtigste Erkenntnis
PA66 drop='path analysis': check where it breaks; weld lines, sharp corners and dry-state brittleness are the three high-incidence areas; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
PA66; drop; weld line; conditioning