Problembeschreibung
The overall color of PA6 products is yellowish, obviously different from the standard color plate
Ursachenanalyse
Excessive melt temperature or excessive residence time causes thermal oxidation yellowing; excessive drying temperature also pre-yellows the pellets, and the two kinds of yellowing need source differentiation; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based only on experience
Lösung
Measure the actual melt temperature not exceeding 270°C; check whether the drying temperature exceeds 100°C; shorten melt residence time; yellowed material must not be used for light-colored products
Wichtigste Erkenntnis
For yellowing, first distinguish whether overheating is in the drying stage or the molding stage, then reduce temperature accordingly; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!