Molds & Tooling 2 Aufrufe

PC Ejection Whitening and Cracking

Problembeschreibung
[Problem Phenomenon] PC whitens and is pushed through at the ejector pins
Ursachenanalyse
Insufficient cooling and low strength, few and small ejector pins, fast ejection; internal stress parts are more prone to ejection cracking; when troubleshooting on site, verify each item according to this mechanism one by one, and avoid blindly adjusting the machine based on experience alone
Lösung
Extend cooling; add ejector pins; reduce the ejection speed; annealing to relieve stress; after adjustment, take samples continuously to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
Wichtigste Erkenntnis
For PC ejection whitening, check cooling and ejection; internal stress parts crack more easily; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
ejection whiteningejector pinscoolingstress