PLA 3D Printing Rough Surface
Problembeschreibung
PLA printed parts have rough surface layer lines, and the appearance and dimensional accuracy are not up to standard
Ursachenanalyse
FDM layer-by-layer deposition inherently has high surface roughness; layer height, nozzle diameter and printing speed jointly determine it; post-treatment (polishing, chemical vapor) can improve it; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
Lösung
①Reduce layer height and optimize speed; ②Mechanical polishing or chemical vapor post-treatment; ③Evaluate other processes for high-precision parts; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
The PLA printing surface is an inherent process attribute; parameter optimization plus post-treatment are the two improvement routes; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence