Material Drying 2 Aufrufe

Bubbles from Insufficient PMMA Drying

Problembeschreibung
Fine bubbles appear inside transparent PMMA parts, and optical parts are directly scrapped.
Ursachenanalyse
PMMA easily absorbs moisture, and moisture-laden pellets vaporize into bubbles at the barrel temperature; transparent parts have zero tolerance for bubbles, and a small amount of moisture can make them visible.
Lösung
①Dry at 80~90℃ for 2~4 hours, reducing the moisture content below 0.05% (stricter for optical parts); ②Dehumidifying drying and verification; ③Seal after drying to prevent rehumidification; ④Section-check the first article for bubbles at startup.
Wichtigste Erkenntnis
PMMA bubbles = drying one-vote veto item.
PMMA; bubbles; drying; moisture content; transparent parts