Molds & Tooling 2 Aufrufe

PMMA Product Ejection Whitening and Puncture

Problembeschreibung
Thin-wall transparent parts are ejection-whitened or even punctured during ejection.
Ursachenanalyse
Insufficient cooling gives low ejection strength, or large shrink-fit force makes local ejector pin pressure exceed the limit; ejection whitening on transparent parts cannot be concealed and they are directly scrapped.; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based on experience alone.
Lösung
①Extend cooling; ②increase ejection area to balance force; ③raise mold temperature to reduce shrink-fit; ④optimize ejector pin layout.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Wichtigste Erkenntnis
The ejection system for transparent parts must be designed to a higher standard; zero tolerance for ejection whitening, and both ejection balance and sufficient cooling are indispensable.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
PMMA; ejection whitening; ejection puncture; ejection; cooling; thin wall