Zurück zu Problem & Lösung
Material Drying 2 Aufrufe

POM surface streaks/silver streaks

Problembeschreibung
Streaks and silver streaks on the product surface.
Ursachenanalyse
Excessively long melt residence causes degradation or trace moisture; although POM has low moisture absorption, both water content and degradation produce surface streaks.
Lösung
①Lower the temperature and clean the barrel; ②pre-dry at 80℃ if necessary; ③shorten residence time; ④check regrind.
Wichtigste Erkenntnis
For POM silver streaks, check degradation first, then moisture.
POM;silver streaks;streaks;degradation;drying