Molds & Tooling 3 Aufrufe

PP Weak Weld Line Strength

Problembeschreibung
Weld lines behind holes of PP parts are obvious, cracking along the weld line under load.
Ursachenanalyse
PP crystallizes fast; if the temperature at the melt front meeting point is insufficient, the crystalline interface bonds weakly; with poor venting, the weld line is more obvious.
Lösung
①Raise melt temperature and injection speed; ②open vent grooves at the meeting point; ③adjust gate position to avoid stressed areas; ④appropriately raise mold temperature to delay front crystallization.
Wichtigste Erkenntnis
PP weld lines must complete entanglement before crystallization.
PP;weld line;crystallization;venting;melt temperature