Problembeschreibung
Parts deform when ejected during demolding, or gradually deform during storage after demolding—unrecoverable, affecting assembly.
Ursachenanalyse
Insufficient cooling time—the part core is ejected before full crystallization and setting; PP crystallizes slowly, especially thick-walled parts; unbalanced ejection, insufficient local part rigidity, and stacking under pressure and heat after demolding also cause secondary deformation.
Lösung
①Extend cooling time to ensure thick walls fully set; ②improve water circuit efficiency and balance mold temperature; ③balance the ejection system and eject at high-rigidity locations; ④pack only after parts fully cool, avoiding stacking pressure and heat; ⑤if necessary, use setting fixtures to constrain cooling.
Wichtigste Erkenntnis
PP 'demolding before setting' is the root of deformation: thick-walled parts need sufficient cooling time and balanced ejection; post-demolding storage and packaging are also high-incidence deformation stages—stacking hot parts equals secondary molding.