PP Ejector Whitening and Cracking

Problembeschreibung
【Problem Phenomenon】PP whitens and is ejected through at ejector pins
Ursachenanalyse
Insufficient cooling and low strength, few and small ejector pins, fast ejection; high incidence in thin walls; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Lösung
Extend cooling; increase ejector pins; reduce ejection speed; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Wichtigste Erkenntnis
For PP ejector whitening check cooling and ejection balance; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future