Problembeschreibung
PSU film extrusion shows uneven thickness and optical defects; high-speed production is difficult; film applications are limited.
Ursachenanalyse
PSU film has high requirements for plasticization uniformity; melt viscosity affects extrusion stability; thickness control accuracy; sensitivity to optical defects.; During on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based solely on experience
Lösung
①Optimize the plasticization system; ②Stabilize extrusion parameters; ③Online thickness measurement control; ④Optical inspection screening.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
PSU film is a high-end application; process stability determines feasibility; online control is a necessary investment.; After confirming effectiveness, solidify the parameters and practices into the work instructions to prevent recurrence