Extrusion & Post 10 Aufrufe

PTFE Filler Segregation

Problembeschreibung
Glass fiber, carbon fiber, or bronze in filled PTFE is unevenly distributed, causing local weakness or uneven wear and inconsistent performance.
Ursachenanalyse
Insufficient mixing of filler and PTFE powder; handling or vibration before molding causes segregation; inconsistent extrusion or compaction causes uneven filler distribution; density differences cause particle separation.
Lösung
①Fully mix filler and PTFE powder to ensure uniformity; ②Handle and store preforms carefully to avoid vibration; ③Optimize extrusion and compaction parameters to ensure uniform filler distribution; ④Sample-check mixing uniformity.
Wichtigste Erkenntnis
PTFE filler segregation affects the uniformity of wear resistance, thermal conductivity, and strength; mixing process is the foundation; handling management is the detail defense line.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PTFE;filler;segregation;mixing;glass fiber;uniformity