Molds & Tooling
3 Aufrufe
PTFE Overheating Degradation
Problembeschreibung
PTFE shows yellowing, carbonization, or smoke release, chemical resistance and mechanical integrity decrease, a safety hazard.
Ursachenanalyse
Sintering temperature exceeding 380℃ causes thermal degradation; local hot spots in ovens, molds, or heaters; prolonged exposure above the recommended temperature upper limit; above 380℃ releases toxic fluoride gases.
Lösung
①Precisely monitor sintering temperature not to exceed 380℃; ②Avoid prolonged exposure to the temperature upper limit; ③Use calibrated thermocouples and uniform heating equipment; ④Ventilation protection for high-temperature operations.
Wichtigste Erkenntnis
PTFE's 380℃ is a double red line of performance and safety; local hot spots are more dangerous than average temperature; toxic gas protection is an occupational health requirement.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
War das hilfreich?
0 Personen fanden dies hilfreich