Menü
Materialien Maschinen
Einblicke
Artikel Videos Problem & Lösung
About
Über Chembull Medienpartner
Kontaktieren Sie uns
Sprache
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Zurück zu Problem & Lösung
Extrusion & Post 10 Aufrufe

PVC Soft Extrusion Temperature

Problembeschreibung
Soft PVC after extrusion shows plasticizer exudation, surface greasy, performance decline
Ursachenanalyse
Soft PVC processing temperature 130-170℃, lower than rigid; too high temperature causes plasticizer volatilization and exudation, surface greasy and material hardens; temperature window needs adjustment by plasticizer content
Lösung
①Soft PVC temperature 130-170℃; ②Prevent local overheating causing plasticizer loss; ③When exudation severe, check formula and temperature matching; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
Soft PVC temperature management must also protect plasticizer; overheating loses not only appearance but also flexibility; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PVC; soft; plasticizer; exudation; 130-170℃

War das hilfreich?

0 Personen fanden dies hilfreich

ChemAI