Molds & Tooling 3 Aufrufe

PVDF Product Flow Marks

Problembeschreibung
Wavy flow marks on the surface.
Ursachenanalyse
Low melt front temperature; slow speed or small gate.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; This mechanism has been repeatedly verified by industry materials, and it should be confirmed first during troubleshooting
Lösung
①Increase temperature; ②increase speed; ③enlarge the gate; ④fill smoothly.; After adjustment, take consecutive samples to verify the effect, and resume mass production only after confirming stability; Change only one variable at a time and record parameter changes, so as to locate effective measures
Wichtigste Erkenntnis
Flow marks are improved by temperature and speed.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; Include this case in the defect archive as a reference for troubleshooting similar problems in the future
PVDF;flow marks;temperature;speed;gate;filling