Molds & Tooling 5 Aufrufe

TPE Product Surface Flow Mark

Problembeschreibung
Wavy flow marks appear on the surface.
Ursachenanalyse
Low front temperature or unstable filling; low mold temperature aggravates flow marks.; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Lösung
①Raise melt and mold temperature; ②optimize the injection speed curve; ③enlarge the gate; ④stable filling.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Wichtigste Erkenntnis
Flow marks are improved by temperature and speed; stable filling is the goal.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
TPE;flow mark;temperature;speed;gate;filling