Extrusion & Post 9 Aufrufe

TPE extrusion roughness

Problembeschreibung
TPE extrusion surface is rough
Ursachenanalyse
Low melt temperature or poor plasticization; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry materials and should be confirmed first during troubleshooting
Lösung
Increase extrusion temperature; ensure plasticization; clean the die head; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
Wichtigste Erkenntnis
For extrusion roughness check temperature and plasticization; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
TPEextrusionroughnessplasticization