Molds & Tooling 3 Aufrufe

TPE ejection whitening

Problembeschreibung
Whitening at the ejector pin positions of TPE products
Ursachenanalyse
Ejection stress concentration; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry materials and should be confirmed first during troubleshooting
Lösung
Enlarge and increase ejector pins; sufficient cooling; sufficient draft; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, so as to locate effective measures
Wichtigste Erkenntnis
Ejection whitening relies on balanced ejection; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
TPEejection whiteningejector pincooling