Problembeschreibung
Melt flowability is extremely poor during injection and extrusion
Ursachenanalyse
High chlorine content leads to stronger intermolecular forces
Lösung
Raise processing temperature by 10-15C and enlarge gates and runners
Wichtigste Erkenntnis
CPVC's high viscosity is the biggest processing challenge