Insufficient drying, silver streaks and bubbles in products
Problembeschreibung
Silver streaks, bubbles on product surface, mechanical properties decline
Ursachenanalyse
Trace moisture vaporizes at high temperature, improper storage management
Lösung
Dehumidifying drying 4-6h, dew point <-30C, moisture <0.05%
Wichtigste Erkenntnis
Must fully dry before processing