Extrusion & Post 9 Aufrufe

Excessive thermal shrinkage of EAA film

Problembeschreibung
The thermal shrinkage of EAA film at 80°C is >12%, exceeding the 5% dimensional stability requirement
Ursachenanalyse
EAA extrusion orientation is released after heating, causing large shrinkage; EAA has a large thermal expansion coefficient; film cooling freezes a large amount of orientation stress
Lösung
1) Reduce the extrusion draw ratio to reduce orientation freezing; 2) Anneal the film at 60-80°C to release orientation stress; 3) Add 5-10wt% rigid resin to reduce thermal shrinkage; 4) Use a biaxial stretching process to balance orientation
Wichtigste Erkenntnis
Film thermal shrinkage is caused by orientation freezing; reducing the draw ratio and annealing treatment are the key
EAA film thermal shrinkage orientation release annealing treatment biaxial stretching

War das hilfreich?

0 Personen fanden dies hilfreich