Material Analysis
10 Aufrufe
Low EAA elongation at break
Problembeschreibung
EAA product elongation at break <100% below the 200% requirement
Ursachenanalyse
EAA molecular weight too low, short chains with insufficient entanglement; excessive orientation causing extremely low transverse elongation; excessive crosslinking restricting chain slippage
Lösung
1) Select high molecular weight EAA to increase entanglement density; 2) Reduce orientation by lowering injection speed; 3) Control crosslinking degree to avoid excess
Wichtigste Erkenntnis
Low elongation at break is caused by low molecular weight and orientation; selecting high MW and reducing orientation is key
War das hilfreich?
0 Personen fanden dies hilfreich
Vielen Dank für Ihr Feedback!