Extrusion & Post
9 Aufrufe
Unstable EEA extrusion dimensions
Problembeschreibung
EEA extruded product cross-section dimensions fluctuate ±10%, with periodic changes along the length direction
Ursachenanalyse
Unstable feeding amount, feeding screw speed fluctuating; extrusion temperature periodically fluctuating ±5°C; haul-off speed not matching extrusion speed
Lösung
1) Use gravimetric feeder to ensure stable feeding; 2) PID control of each extruder section temperature with accuracy ±1°C; 3) Closed-loop control of haul-off speed linked with extrusion speed; 4) Control processing temperature at 160-210±5°C
Wichtigste Erkenntnis
Extrusion dimensional stability depends on feeding accuracy, temperature control and haul-off synchronization