Extrusion & Post 10 Aufrufe

EMA Film Poor Printing Adhesion

Problembeschreibung
After printing on EMA film, ink adhesion
Ursachenanalyse
Poor affinity between EMA surface polarity and ink; corona treatment effect decays fast; ink system does not match EMA
Lösung
1) Print immediately after corona treatment, within 24h; 2) Use EMA-specific ink; 3) Increase corona power to 15-20kW/m² to ensure surface tension >42mN/m; 4) Flame treatment to assist surface polarization
Wichtigste Erkenntnis
Poor printing adhesion is caused by insufficient surface polarity; corona treatment and special ink are key
EMA film printing adhesion corona treatment special ink surface tension