Material Analysis 10 Aufrufe

Poor EMA chemical resistance

Problembeschreibung
After soaking EMA products in acid, alkali or solvent, mechanical properties decline >30%
Ursachenanalyse
EMA has high affinity for specific chemicals and is attacked and swelled; EMA molecular chains attacked by chemicals and broken
Lösung
1) Select chemical resistant grade; 2) Slight crosslinking to reduce swelling; 3) Product surface coating protection; 4) Add chemical stabilizer
Wichtigste Erkenntnis
Poor chemical resistance is caused by EMA chemical affinity; selecting chemical resistant grade and coating are key
EMA chemical resistance chemical attack slight crosslinking surface coating