Material Analysis 14 visualizações

Poor EMA chemical resistance

Fenómeno do problema
After soaking EMA products in acid, alkali or solvent, mechanical properties decline >30%
Análise das causas
EMA has high affinity for specific chemicals and is attacked and swelled; EMA molecular chains attacked by chemicals and broken
Solução
1) Select chemical resistant grade; 2) Slight crosslinking to reduce swelling; 3) Product surface coating protection; 4) Add chemical stabilizer
Conclusão principal
Poor chemical resistance is caused by EMA chemical affinity; selecting chemical resistant grade and coating are key
EMA chemical resistance chemical attack slight crosslinking surface coating