EVA foam density is too high
Problembeschreibung
EVA foamed shoe material density 0.35 is higher than 0.25g/cm³
Ursachenanalyse
Insufficient AC or incomplete decomposition; VA<15% high viscosity suppresses expansion; insufficient crosslinking
Lösung
1) AC 0.8-1.2wt%; 2) VA18-28% to reduce viscosity and promote expansion; 3) Foaming at 170-180°C; 4) DCP 0.4-0.6wt% to stabilize cells
Wichtigste Erkenntnis
EVA foam density is determined by the blowing agent, VA content, and crosslinking degree