Material Analysis 9 views

EVA foam density is too high

Problem Phenomenon
EVA foamed shoe material density 0.35 is higher than 0.25g/cm³
Cause Analysis
Insufficient AC or incomplete decomposition; VA<15% high viscosity suppresses expansion; insufficient crosslinking
Solution
1) AC 0.8-1.2wt%; 2) VA18-28% to reduce viscosity and promote expansion; 3) Foaming at 170-180°C; 4) DCP 0.4-0.6wt% to stabilize cells
Key Takeaway
EVA foam density is determined by the blowing agent, VA content, and crosslinking degree
EVA foam high density AC blowing agent VA content DCP crosslinking