Processing Machinery 3 Aufrufe

EVA material changeover residue

Problembeschreibung
After EVA material changeover, the first 5-10 products contain residue of the previous material with color difference and performance deviation
Ursachenanalyse
Large amount of previous material residue in the barrel and screw; incomplete purging with residue in dead zones; insufficient purging compound amount
Lösung
1) Increase purging compound amount to 2-3 times the barrel capacity; 2) Increase rotation speed and temperature during purging to accelerate removal; 3) Disassemble the screw to thoroughly clean dead zones
Wichtigste Erkenntnis
Changeover residue is caused by incomplete purging; thorough purging and disassembly are key
EVA changeover residue purging compound screw disassembly dead zone cleaning