문제 현상
After EVA material changeover, the first 5-10 products contain residue of the previous material with color difference and performance deviation
원인 분석
Large amount of previous material residue in the barrel and screw; incomplete purging with residue in dead zones; insufficient purging compound amount
해결 방법
1) Increase purging compound amount to 2-3 times the barrel capacity; 2) Increase rotation speed and temperature during purging to accelerate removal; 3) Disassemble the screw to thoroughly clean dead zones
핵심 요약
Changeover residue is caused by incomplete purging; thorough purging and disassembly are key