Molds & Tooling 3 Aufrufe

EVA internal shrinkage voids

Problembeschreibung
Shrinkage voids of 0.5-2mm diameter in the center of thick-walled EVA products
Ursachenanalyse
After cooling of thick-wall areas the interior shrinks but the surface has solidified and cannot be fed; holding time insufficient with the gate freezing too early
Lösung
1) Extend holding time until the gate is completely frozen; 2) Increase gate size to delay freezing; 3) Product design to reduce wall thickness differences
Wichtigste Erkenntnis
Shrinkage voids are caused by thick-wall shrinkage and insufficient holding; extending holding is key
EVA shrinkage void thick wall holding time gate freezing

War das hilfreich?

0 Personen fanden dies hilfreich

ChemAI