Molds & Tooling
3 Aufrufe
Poor EVOH Surface Gloss
Problembeschreibung
EVOH product surface gloss <60%, below the 80% requirement, dull appearance
Ursachenanalyse
Mold surface rough Ra>0.4μm; EVOH crystallinity high, surface microcrystals scatter light; cooling rate improper
Lösung
1) Polish mold to Ra<0.1μm mirror finish; 2) Increase mold temperature to delay crystallization and reduce scattering; 3) Add nucleating agent to control crystal size
Wichtigste Erkenntnis
Poor gloss is caused by mold roughness and crystalline scattering; polishing mold and controlling crystallization are key
War das hilfreich?
0 Personen fanden dies hilfreich