Processing Machinery 3 Aufrufe

Internal unmelted particles of PU

Problembeschreibung
Unmelted transparent or translucent particles appear inside PU products
Ursachenanalyse
Screw plasticizing capacity insufficient, temperature too low; feed amount too large, exceeding plasticizing capacity; PU melting temperature too high
Lösung
1) Increase processing temperature to ensure full melting; 2) Reduce feed amount to match plasticizing capacity; 3) Increase screw mixing section
Wichtigste Erkenntnis
Unmelted particles are caused by insufficient plasticizing; increasing temperature and reducing feeding are key
PU unmelted particles plasticizing capacity processing temperature screw mixing