Processing Machinery
8 visualizaciones
Internal unmelted particles of PU
Fenómeno del problema
Unmelted transparent or translucent particles appear inside PU products
Análisis de la causa
Screw plasticizing capacity insufficient, temperature too low; feed amount too large, exceeding plasticizing capacity; PU melting temperature too high
Solución
1) Increase processing temperature to ensure full melting; 2) Reduce feed amount to match plasticizing capacity; 3) Increase screw mixing section
Conclusión clave
Unmelted particles are caused by insufficient plasticizing; increasing temperature and reducing feeding are key