PU hardness too low

Problembeschreibung
PU product Shore hardness 5-10 degrees lower than target, soft to touch
Ursachenanalyse
PU soft nature, low hardness; too much plasticizer or softener added; crystallinity too low
Lösung
1) Add rigid filler 5-10wt% to increase hardness; 2) Reduce plasticizer dosage; 3) Increase cooling rate to increase crystallinity
Wichtigste Erkenntnis
Low hardness is caused by material softness and excessive plasticization; adding filler is key
PU low hardness rigid filler plasticizer crystallization control