PU hardness too low
문제 현상
PU product Shore hardness 5-10 degrees lower than target, soft to touch
원인 분석
PU soft nature, low hardness; too much plasticizer or softener added; crystallinity too low
해결 방법
1) Add rigid filler 5-10wt% to increase hardness; 2) Reduce plasticizer dosage; 3) Increase cooling rate to increase crystallinity
핵심 요약
Low hardness is caused by material softness and excessive plasticization; adding filler is key