Injection Molding
2 Aufrufe
Severe excessive orientation of PU
Problembeschreibung
Longitudinal-transverse performance difference of PU products >50%, excessive orientation
Ursachenanalyse
Injection speed too fast, molecular chains highly oriented in the flow direction; gate design causing unidirectional flow
Lösung
1) Reduce injection speed to reduce orientation; 2) Multi-point gates to reduce unidirectional flow; 3) Annealing treatment to partially release orientation
Wichtigste Erkenntnis
Excessive orientation is caused by fast unidirectional flow; speed reduction and multi-point gates are key