Injection Molding 7 visualizaciones

Severe excessive orientation of PU

Fenómeno del problema
Longitudinal-transverse performance difference of PU products >50%, excessive orientation
Análisis de la causa
Injection speed too fast, molecular chains highly oriented in the flow direction; gate design causing unidirectional flow
Solución
1) Reduce injection speed to reduce orientation; 2) Multi-point gates to reduce unidirectional flow; 3) Annealing treatment to partially release orientation
Conclusión clave
Excessive orientation is caused by fast unidirectional flow; speed reduction and multi-point gates are key
PU excessive orientation injection speed multi-point gates performance difference

¿Le ha resultado útil?

0 personas encontraron esto útil