Material Analysis 10 Aufrufe

Fast PVA thermal aging

Problembeschreibung
PVA product aged at 80°C for 7 days, mechanical properties decrease >30%
Ursachenanalyse
PVA molecular chains break and degrade under thermal oxidation; antioxidant system incomplete, insufficient protection
Lösung
1) Improve the antioxidant system 1010+168+DSTDP; 2) Select high molecular weight grade; 3) Add metal deactivator 0.05wt%
Wichtigste Erkenntnis
Thermal aging is caused by thermal oxidation; improving the antioxidant system is the key
PVAthermal agingthermal oxidationantioxidanthigh molecular weight